Skip to Main text

Surface Protective Materials SPV™-3620K

Surface protective materials for machine processing.

SPV-3620K is a surface protective materials of polyethylene film base. With its moderate adhesion, good adhesive for rough surfaces.

Download

Features

  • Changes in adhesive strength after lamination are extremely small, ensuring easy peeling.
  • Minimally affected by surface condition (roughness) of the substrate, applicable for a wide range of substrates.
  • Withstand light processing such as shallow drawing and bending, preventing damage during processing.
  • Light unwinding force offers easy laminating.

Properties

Product No. Thickness[mm]*1 Adhesive strength[N/20mm]*2
SPV™-3620K 0.070 2.30

[Test method]

  • *1:Nominal thickness
  • *2:Peeling angle: 180°, Peeling speed: 300mm/min

Applications

  • Surface protective for melamine plywood, pre-coated plates and plastic plates during storage, transportation, and processing.

Precautions

  • Avoid sunlight and store at room temperature and moderate humidity.
  • Do not press too strong when applying. This may cause the end of the tape to peel.
  • If applying to surfaces treated with machining oil, degrease the surface carefully. Any remains will be a cause for surface contamination or adhesive residue.
  • For use under severe conditions, please test and evaluate the product thoroughly beforehand.
  • Painting, plating, etching, or gluing the surface after peeling the tape may be troublesome due to the small amount of residue of the adhesive. Please inspect under actual situations thoroughly before application.
  • Painted boards, depending on conditions such as paint baking, may cause the tape to peel uneasily or peel off the paint together. Please evaluate thoroughly beforehand.
  • Surface treated boards such as alumite, depending on treatment conditions, may show different properties (peeling) of SPV. Please evaluate thoroughly beforehand.
  • Especially for applications against natural substrate (marble stone, lumber, etc.) please contact our sales representative in charge.
  • Painting after peeling off SPV-3620K could cause the repellency of the paint or insufficient paint adhesion.
  • When you paint after peeling off the surface protective material, be sure to check the surface washing, pretreatment, or paint baking conditions to ensure the paint adhesion before usage.

  • The above datasheet is a sample observation value under certain testing conditions, not guaranteed performance.
  • The quality, performance, and/or functions of this product will differ according to the conditions of use. Please contact our department in charge for full details of this product.
  • Under severe conditions, this product may show difference between the sample observed values and the actual performance. Please test and evaluate the product thoroughly for your safety and better results.
  • This product and/or its features may change or be discontinued without any prior notice.
  • The intellectual property rights of this document belongs to Nitto Denko Corporation. Please contact our department in charge for usage not in accordance of the intended use. Copying and/or reproducing the document without notice are strictly prohibited. All rights reserved.

Contact Us

For inquiries about products.

Business Hours(Japan time) 9:00-17:30 Except for Sat, Sun, and Holidays

Global Site